Metals

MS / Mild Steel

Economical general-purpose carbon steel

Density
7.85 g/cm³
Tensile
340-450 MPa
Max T
400 °C
Strength
52
Lightness
25
Heat
55
Metals

S235JR

Common structural steel for fabrication

Density
7.85 g/cm³
Tensile
360-510 MPa
Max T
400 °C
Strength
50
Lightness
25
Heat
55
Metals

S275JR

Structural steel with improved strength

Density
7.85 g/cm³
Tensile
370-530 MPa
Max T
~400 °C
Strength
56
Lightness
25
Heat
55
Metals

S355JR / S355J2

High-strength structural steel

Density
7.85 g/cm³
Tensile
470-630 MPa
Max T
~400 °C
Strength
66
Lightness
25
Heat
55
Metals

EN8

Medium-carbon steel for machined parts

Density
7.85 g/cm³
Tensile
550-800 MPa
Max T
~400 °C
Strength
68
Lightness
25
Heat
55
Metals

EN9

Carbon steel for stronger machine parts

Density
7.85 g/cm³
Tensile
600-850 MPa
Max T
~400 °C
Strength
72
Lightness
25
Heat
55
Metals

EN19

Alloy steel for high-strength components

Density
7.85 g/cm³
Tensile
850-1100 MPa
Max T
~400 °C
Strength
84
Lightness
25
Heat
58
Metals

EN24

High-strength alloy steel for critical parts

Density
7.85 g/cm³
Tensile
900-1200 MPa
Max T
~400 °C
Strength
88
Lightness
25
Heat
58
Metals

SS 303

Free-machining stainless steel

Density
7.9 g/cm³
Tensile
500-750 MPa
Max T
~800 °C
Strength
64
Lightness
28
Heat
82
Metals

SS 304

General-purpose stainless steel

Density
8.0 g/cm³
Tensile
520-750 MPa
Max T
~800 °C
Strength
66
Lightness
28
Heat
82
Metals

SS 304L

Low-carbon stainless for welding

Density
8.0 g/cm³
Tensile
500-700 MPa
Max T
~800 °C
Strength
62
Lightness
28
Heat
82
Metals

SS 316

Marine-grade stainless steel

Density
8.0 g/cm³
Tensile
515-760 MPa
Max T
~800 °C
Strength
68
Lightness
28
Heat
82
Metals

SS 316L

Low-carbon marine-grade stainless

Density
8.0 g/cm³
Tensile
500-720 MPa
Max T
~800 °C
Strength
66
Lightness
28
Heat
82
Metals

SS 430

Ferritic stainless for sheet applications

Density
7.7 g/cm³
Tensile
450-600 MPa
Max T
~800 °C
Strength
58
Lightness
30
Heat
82
Metals

SS 17-4 PH / 630

Precipitation-hardening stainless steel

Density
7.75 g/cm³
Tensile
900-1200 MPa
Max T
~600 °C
Strength
88
Lightness
30
Heat
70
Metals

Duplex 2205

High-strength duplex stainless steel

Density
7.8 g/cm³
Tensile
620-900 MPa
Max T
300-600 °C
Strength
78
Lightness
30
Heat
72
Metals

Aluminium 1050

Commercially pure aluminium

Density
2.71 g/cm³
Tensile
70-120 MPa
Max T
~200 °C
Strength
24
Lightness
88
Heat
35
Metals

Aluminium 5052

Formable aluminium with marine resistance

Density
2.68 g/cm³
Tensile
190-260 MPa
Max T
~150-200 °C
Strength
42
Lightness
89
Heat
38
Metals

Aluminium 5083

Marine-grade aluminium plate

Density
2.66 g/cm³
Tensile
275-350 MPa
Max T
~200 °C
Strength
50
Lightness
90
Heat
40
Metals

Aluminium 5754

Good forming and welding aluminium

Density
2.66 g/cm³
Tensile
190-330 MPa
Max T
~150-200 °C
Strength
44
Lightness
90
Heat
38
Metals

Aluminium 6060

Extrusion-friendly aluminium alloy

Density
2.70 g/cm³
Tensile
150-220 MPa
Max T
~150 °C
Strength
36
Lightness
88
Heat
35
Metals

Aluminium 6061

Versatile machinable aluminium alloy

Density
2.70 g/cm³
Tensile
240-310 MPa
Max T
~150-200 °C
Strength
52
Lightness
88
Heat
42
Metals

Aluminium 6082

Structural aluminium for machined parts

Density
2.70 g/cm³
Tensile
250-350 MPa
Max T
~150-200 °C
Strength
56
Lightness
88
Heat
42
Metals

Aluminium 7075

High-strength aerospace aluminium

Density
2.81 g/cm³
Tensile
500-600 MPa
Max T
~120 °C
Strength
78
Lightness
86
Heat
32
Metals

Brass

Machinable copper-zinc alloy

Density
8.40-8.70 g/cm³
Tensile
250-600 MPa
Max T
~200-300 °C
Strength
52
Lightness
18
Heat
45
Metals

Free-cutting Brass

Precision brass for turned parts

Density
8.40-8.70 g/cm³
Tensile
300-500 MPa
Max T
~200-300 °C
Strength
50
Lightness
18
Heat
45
Metals

Naval Brass

Marine brass for fittings and hardware

Density
8.40-8.60 g/cm³
Tensile
350-500 MPa
Max T
~200-300 °C
Strength
52
Lightness
18
Heat
45
Metals

Cartridge Brass

Formable brass for stamped parts

Density
8.40-8.60 g/cm³
Tensile
300-500 MPa
Max T
~200-300 °C
Strength
50
Lightness
18
Heat
45
Metals

Copper

High-conductivity pure metal

Density
8.94 g/cm³
Tensile
200-400 MPa
Max T
~200-250 °C
Strength
42
Lightness
16
Heat
48
Metals

Electrolytic Copper

High-purity conductive copper

Density
8.94 g/cm³
Tensile
200-400 MPa
Max T
~200-250 °C
Strength
42
Lightness
16
Heat
48
Metals

Oxygen-free Copper

Premium copper for electronics and vacuum use

Density
8.94 g/cm³
Tensile
200-400 MPa
Max T
~200-250 °C
Strength
42
Lightness
16
Heat
48
Metals

Bronze

Durable copper alloy for wear parts

Density
8.70-8.90 g/cm³
Tensile
200-500 MPa
Max T
~250-300 °C
Strength
50
Lightness
17
Heat
50
Metals

Phosphor Bronze

Springy bronze alloy for precision parts

Density
8.80-8.90 g/cm³
Tensile
300-700 MPa
Max T
~250-300 °C
Strength
62
Lightness
17
Heat
50
Metals

Aluminium Bronze

High-strength bronze for marine wear parts

Density
7.60-8.30 g/cm³
Tensile
500-900 MPa
Max T
~300 °C
Strength
72
Lightness
20
Heat
52
Metals

Gunmetal / Tin Bronze

Cast bronze for valves and pump parts

Density
8.70-8.90 g/cm³
Tensile
200-500 MPa
Max T
~250-300 °C
Strength
50
Lightness
17
Heat
50
Metals

Ti-6Al-4V Titanium

Aerospace-grade strength to weight

Density
4.43 g/cm³
Tensile
950 MPa
Max T
400 °C
Strength
92
Lightness
78
Heat
80
Engineering Plastics

PEEK (Polyetheretherketone)

Metal-replacement thermoplastic

Density
1.32 g/cm³
Tensile
100 MPa
Max T
260 °C
Strength
70
Lightness
92
Heat
85
Engineering Plastics

ABS

Tough, prototyping friendly

Density
1.05 g/cm³
Tensile
40 MPa
Max T
90 °C
Strength
45
Lightness
88
Heat
35
Composites

Carbon Fiber Composite

Best-in-class stiffness to weight

Density
1.6 g/cm³
Tensile
1500 MPa
Max T
150 °C
Strength
95
Lightness
96
Heat
65
Ceramics

Alumina (Al₂O₃)

Hard, electrically insulating

Density
3.95 g/cm³
Tensile
300 MPa
Max T
1700 °C
Strength
60
Lightness
40
Heat
98
Elastomers

Silicone Elastomer

Flexible, biocompatible

Density
1.15 g/cm³
Tensile
9 MPa
Max T
230 °C
Strength
20
Lightness
80
Heat
85
Advanced Manufacturing

PA12 (SLS Nylon)

Production-grade 3D printing

Density
1.01 g/cm³
Tensile
48 MPa
Max T
170 °C
Strength
55
Lightness
90
Heat
55
Back to AmorphousIndia.com